SGC440 asye bobin / teren / fèy tretman sifas:
C (tretman chromat), NC (tretman ki pa chromat), O (lwilizasyon), X (unoiling) NP (tretman fosfat ki pa chromat), P (fosfat), M (ki pa trete)
SGC440 asye bobin / teren / fèy kouch mas:
Pi Zenk kouch: Z06 (60g), Z08 (80g), Z10 (100g), Z12 (120g), Z14 (140g), Z18 (180g), Z20 (200g), Z22 (220g), Z25 (250g), Z27 (270g), Z35 (350g), Z37 (370g), Z45 (450g), Z60 (450g)
Alyaj Zenk + Fe: F04 (40g), F06 (60g), F08 (80g), F10 (10g0), F12 (120g), F18 (180g)
SGC440 asye bobin / teren / fèy kouch: Z (Pure Zenk), ZF (Z + Fe alyaj)
JIS G 3302 SGC440 asye gwosè apwopriye: epesè 0.25mm -3.2mm
SGC440 asye konpozisyon chimik %:
| Klas | C max | Mn max | P max | S max |
| SGC440 | 0.25 | 2.0 | 0.20 | 0.05 |
SGC440 asye asye Pwopriyete mekanik
| Klas | Sede fòs MPa | Fòs rupture MPa | Elongasyon % min | |||||
| {{0}}.25- Mwens pase oswa egal a 0.40mm | {{0}}.40- Mwens pase oswa egal a 0.60mm | {{0}}.60- Mwens pase oswa egal a 1.0mm | 1.0- Mwens pase oswa egal a 1.6mm | 1.6- Mwens pase oswa egal a 2.5mm | Pi wo pase 2.5mm | |||
| SGC440 | 335 min | 440 min | 18 | 18 | 18 | 18 | 18 | 18 |
GNEE STEEL gen plis pase 2000 tòn SGC440 sous stock asye chak mwa. Nou ka rankontre pi fò kliyan nou an nan kantite ak demann teknik. Ki baze sou sous stock sa yo, endistri avantaj nou an gaye nan pwosesis asye tankou: koupe (sou lajè ak longè), desen, remballage, ak sou sa.

Baj popilè: sgc440 plonje cho galvanised asye, Lachin sgc440 plonje cho galvanised asye manifaktirè, Swèd, faktori